Last updated:

How to fix Z-banding (horizontal lines on 3D prints)

Your print is the right shape, but the walls have stripes: ridges or darker lines running all the way around at regular heights. That's usually called Z-banding. Before you start taking the printer apart, it's worth working out which kind of line you have, because a single line at one height and repeating stripes up the whole print have different causes. Work down this list in order, cheapest checks first.

First, which lines do you have?

What you seeWhat it usually isWhere to start
Fine, even lines, every one the sameNormal layer linesNothing is wrong. Use a smaller layer height if you want a smoother look
One line at one height (for example around a Benchy's hull)A change inside the model at that layerStep 1: check the slicer preview
Stripes repeating up the whole print, all the way aroundZ-banding: uneven Z movement or extrusionSteps 2 to 6
Ripples after corners and letters, along the wallNot banding: vibrationFix ghosting and ringing
Whole layers moved sidewaysNot banding: layer shiftFix layer shifting
Hold the print up to a light and turn it slowly. Banding catches the light all the way around. Lines on just one side, or that follow the corners, usually point to something else.

Step 1: Check the slicer preview for that height

A single line at one height is very often caused by the slicer, not the printer. Prusa has a whole article on the "Benchy hull line", the ridge many people see around the hull of the 3DBenchy test boat (from our first things to print list). Prusa's explanation is that the main culprit is the sudden switch from sparse infill to solid top layers around 8 mm up: suddenly each layer takes much longer to print, then a few layers later it's quick again. That change in timing and cooling shows on the outside wall.

Step 2: Clean and grease the Z lead screws

The lead screws are the long threaded rods that move the bed (or the whole print head gantry) up between layers. Dust, bits of plastic and old, gritty grease can make them move unevenly, so some layers end up slightly taller or shorter than others. This is the most common mechanical cause and the easiest to fix.

Only put grease where your maker says. Bambu Lab, for example, says no oil or grease on the X-axis carbon rods of the X1 and P1 series, and no grease on the A1's X-axis linear rail.

Step 3: Make sure nothing is binding

If something rubs or catches while the Z axis moves, it can stick for a moment and then jump, leaving a line. With the printer off or idle, watch the bed or gantry move up and down using the printer's move controls and look for:

Bambu Lab's wiki lists things like debris on the Z sliders, the heat bed cable dragging and the bed hitting the purge chute as reasons the Z axis can catch. Clear anything you find, then reprint the same model.

One fix a week, in plain English

Join The First Layer, our free beginner email. Each issue solves one common problem like this one. New subscribers get the free First Print Checklist.

No spam, unsubscribe any time. See our privacy policy.

Step 4: Rule out uneven extrusion

Not all banding comes from the Z axis. If the amount of plastic coming out of the nozzle surges and dips, some layers end up fatter than others, and that looks like stripes too.

Step 5: Keep cooling and the room steady

If the air around the print keeps changing, from a fan switching on, an air conditioner or an open window, layers cool at different speeds and can come out slightly different sizes. Keep the printer out of drafts, close the door on enclosed printers, and leave part cooling at your filament profile's default unless you have a reason to change it.

Step 6: Older printers: try a "full step" layer height

On many older and budget printers, the Z axis is driven by a stepper motor turning a lead screw, and it moves most evenly when each layer is a whole number of the motor's full steps. A common setup is a motor with 200 full steps per turn and a lead screw that moves 8 mm per turn, which works out to 0.04 mm per full step. On those printers, layer heights that are multiples of 0.04 mm (0.12, 0.16, 0.2, 0.24 mm) can band less than in-between values like 0.15 mm. Check your printer's specs for its own numbers. Most current printers' default profiles already use layer heights like 0.2 mm, so this matters mainly if you've typed in your own.

Quick reference: what to try

What you seeLikely causeTry this
One line where the infill turns solidChange in layer time and coolingCheck the preview, slow outer walls, keep cooling steady
Stripes up the whole print, Z axis sounds dry or squeakyDirty or dry lead screwsClean and grease the lead screws
Lines at the same heights on every printSomething catching at that heightWatch the Z axis move, clear cables and debris
Rough, uneven walls plus popping soundsWet filamentDry the filament
Bands only with an unusual layer height on an older printerLayer height between motor stepsUse 0.12, 0.16, 0.2 or 0.24 mm

Sources

Checked October 28, 2026: Prusa Knowledge Base, The Benchy hull line and Regular printer maintenance (XL); Bambu Lab Wiki, X1 Maintenance Recommendation, P1 series Maintenance Recommendation, A1 Maintenance Guidelines, Lubricant Grease and Lubricant Oil and Z axis motor stuck (HMS code).

Your next step

Find the height of your worst line and check the slicer preview there first. If nothing changes at that layer, clean and grease the lead screws following your printer maker's guide, and reprint the same model so you can compare. If the walls are rough as well as striped, dry your filament before you change anything else.

Frequently asked questions

What is Z-banding in 3D printing?

Z-banding is a pattern of horizontal lines or ridges that run around the outside of a print at regular heights, so the wall looks striped instead of smooth. It happens when some layers come out slightly fatter, thinner or shifted compared with the layers around them, usually because the Z axis (the part that moves up between layers) is not moving perfectly evenly, or because extrusion is surging and dipping.

Is Z-banding the same as normal layer lines?

No. Every FDM print has fine, even layer lines because it is built one layer at a time. Z-banding is when some of those lines stand out from the rest in a repeating pattern, like thicker stripes every few millimeters. If every line looks the same, that is just layer height, and a smaller layer height makes it finer.

Why is there one line around my Benchy at the same height?

That is usually not Z-banding. Prusa calls it the Benchy hull line and says the main cause is the sudden change from sparse infill to solid top layers around 8 mm up, which changes how long each layer takes and how the plastic cools. A single line at a height where the inside of the model changes points to slicer settings and cooling, not to the lead screws.

How often should I grease my Z lead screws?

Follow your printer maker. Bambu Lab recommends checking and greasing the Z lead screws every three months on the X1, P1 and A1 series. Prusa recommends lubricating the Z leadscrews on the XL after about 500 hours of printing. Clean off old grease and dust first, and use a thin coat of grease, not a thick blob.

Can wet filament cause horizontal lines?

It can make them worse. Damp filament pops and bubbles as it is heated, so the amount of plastic coming out of the nozzle changes from moment to moment. That shows up as rough, uneven walls and can look like bands. Drying the filament is a cheap thing to rule out before you take anything apart.

One short, friendly email a week: one fix or lesson, one honest pick, and one fun thing to print. New subscribers get the free First Print Checklist.