Last updated:
How to print PETG: beginner settings and tips that work
PETG is the natural next step after PLA: tougher, more heat resistant, and still easy enough for a beginner. Prusa even uses it for parts of its own printers. But if you load it with your PLA habits, you'll probably get strings, blobs and maybe a print welded to the bed. This guide walks through the switch in order, so your first PETG print works.
Not sure you need PETG yet? Read PLA vs PETG for beginners first. Short version: use PETG for parts that bend, get knocked around, or sit somewhere warm like a car.
PETG vs PLA settings at a glance
These are typical reference numbers from Prusa and Bambu Lab. Always check the range printed on your spool, since brands differ.
| Setting | PLA (for comparison) | PETG |
|---|---|---|
| Nozzle temperature | About 190 to 230 °C | About 230 to 250 °C (Prusa: 230 °C first layer, 240 °C after) |
| Bed temperature | About 35 to 65 °C | About 60 to 90 °C (Bambu Lab: 60 to 80 °C; Prusa: 85 to 90 °C) |
| Build plate | Almost anything | Textured PEI. Smooth PEI only with glue stick |
| Part cooling fan | High | Lower; Prusa suggests fan off for the first layers, then about half |
| First-layer height | Pressed in slightly | A touch higher, not squished |
| Drying | When it acts wet | Before the first print, and store it sealed |
Step 1: Dry the spool first
PETG soaks up moisture from the air much faster than PLA. Bambu Lab calls it highly hygroscopic and says damp PETG causes stringing, bubbles, rough surfaces and weak parts, because the water boils inside the nozzle. Even a brand-new spool can arrive damp.
- Bambu Lab's numbers: 60 to 65 °C for 8 hours in a convection dryer, or 80 °C for 12 hours on a printer's heated bed with the spool covered.
- Afterwards, keep it in a sealed bag or box with desiccant (the little drying packets).
- Full how-to, including how to tell if a spool is wet: how to dry 3D printer filament.
Step 2: Use a real PETG profile in your slicer
The slicer is the program that turns your model into printer instructions. Don't just raise the temperature on your PLA profile. Pick the PETG profile for your brand if your slicer has one, or the generic PETG profile. Those already set the right temperatures, slower fan, retraction and speed limits. Prusa's own advice for PETG stringing is to start from the PrusaSlicer profiles rather than tuning everything by hand, and the same idea applies in Bambu Studio, OrcaSlicer and Cura.
Step 3: Choose the right build plate (and use glue if needed)
This is the step that catches most people. PETG grips some surfaces so hard that removing the print tears the plate.
- Textured PEI (the rough, sparkly sheet that comes with many printers, including Bambu Lab's): works well, usually with no glue. Bambu Lab says to add a thin layer of glue if PETG prints are hard to get off.
- Smooth PEI: Prusa warns that PETG can stick too well and damage it. If it's all you have, wipe on a thin layer of glue stick first. Here the glue is a release layer, not for extra grip.
- PLA-only "cool" plates: Bambu Lab says its discontinued Cool Plate is only suited to PLA; PETG can bulge and stick on it.
Whatever plate you use, wash it with dish soap and water first. Finger grease is the most common reason any first layer won't stick. See first layer not sticking if it still won't hold.
Step 4: Don't squish the first layer
With PLA, a first layer pressed a little into the bed is great. With PETG, a nozzle that's too close scrapes up the sticky plastic, builds blobs on the nozzle and drags them across the print. Many people raise the first layer very slightly for PETG compared with PLA. If you're not sure how to adjust that, read how to level a 3D printer bed, which covers the Z offset (the fine height setting for the first layer).
Watch the first layer go down. You want lines that touch each other and look slightly flattened, not ridged, transparent or plowed.
One fix a week, in plain English
Join The First Layer, our free beginner email. Each issue solves one common problem like this one. New subscribers get the free First Print Checklist.
No spam, unsubscribe any time. See our privacy policy.
Step 5: Less cooling, steadier speed
- Cooling: PETG needs less fan than PLA. Prusa suggests the first few layers with the fan off, then about half power. More fan gives sharper detail; less fan gives stronger layer bonding.
- Speed: if you see blobs, rough patches or bumps on the walls, slow down. Bambu Lab notes that extrusion is more stable at lower speed and suggests about 90 mm/s for outer surfaces when this happens. If you slow down a lot, lower the nozzle temperature a little too, since the plastic has more time to heat.
- Overhangs and bridges droop more in PETG. See how to fix droopy overhangs.
Step 6: Remove the print the right way
Let the plate cool down fully, then flex it. Bambu Lab recommends waiting until the plate is at about 35 °C or cooler before removing prints from PEI. Prying a hot PETG print off with a scraper is how plates get gouged. Still stuck? See how to get a print stuck to the bed off.
Common PETG problems and quick fixes
| What you see | Likely cause | Try this |
|---|---|---|
| Fine hairs and strings everywhere | Damp filament or nozzle too hot | Dry the spool, then lower the nozzle 5 °C. More in fix stringing |
| Blobs stuck to the nozzle and dragged across the print | First layer too close, or oozing | Raise the first layer slightly, clean the nozzle, slow down |
| Bubbles, popping sounds, rough walls | Wet filament | Dry it before anything else |
| Print welded to the plate or pulled chunks out | Smooth PEI with no release layer | Glue stick on smooth PEI, or switch to textured PEI; remove only when cool |
| Corners lifting on big flat parts | Uneven cooling | Add a brim, block drafts. See fix warping |
| Weak layers that split apart | Too cold or too much fan | Raise the nozzle 5 °C, lower the fan. A temperature tower finds the sweet spot |
| Clogs partway through | Flow or temperature too high for the speed | Use the default profile and see fix a clogged nozzle |
Want stronger PETG parts?
PETG is popular for functional parts, so strength matters. Prusa suggests adding more walls (perimeters) rather than more infill for solid parts. Bambu Lab adds that you should think about which way the part will be pushed or pulled, and orient it so that force doesn't try to split the layers apart, since layers are the weakest direction of any print.
Sources
Checked October 30, 2026: Prusa Knowledge Base, PETG; Bambu Lab Wiki, PETG Usage Guide, Filament guide material table, How to use Bambu Lab glue and Introduction to Bambu Lab Build Plates.
Your next step
Dry your PETG spool tonight, load your slicer's PETG profile, and print something small and useful, like a hook or clip from our first things to 3D print list. If it strings, dry it again before you touch any settings. Once it works, you have a filament for tough, heat-resistant parts.
Frequently asked questions
What temperature should I print PETG at?
Use the range printed on your spool. As a reference, Prusa recommends 230 °C for the first layer and 240 °C after that with a bed of 85 to 90 °C, and Bambu Lab lists 60 to 80 °C for the bed on its textured PEI plate. To find the best nozzle temperature for your own spool, print a temperature tower.
Do I need glue stick for PETG?
Not on a textured PEI plate in most cases. On a smooth PEI plate, yes: PETG can stick so hard that it pulls pieces out of the surface, so Prusa recommends a thin layer of glue stick as a release layer. Bambu Lab also suggests glue on a textured plate if PETG prints are hard to remove.
Why is my PETG so stringy?
Usually because the spool has absorbed moisture, or the nozzle is too hot. Bambu Lab calls PETG highly hygroscopic (it soaks up water from the air) and says obvious stringing is a sign the filament is damp. Dry it first, then try lowering the nozzle temperature by 5 °C.
Does PETG need an enclosure?
No. PETG warps much less than ABS and prints fine on an open printer. Keep drafts away, and use a brim on large flat parts if corners lift.
Is PETG food safe?
Do not assume so. Bambu Lab says its PETG filaments are not food-contact grade, and Prusa does not recommend any 3D printed part for direct food contact because bacteria can grow in the tiny grooves between layers.
Why does PETG stick to my nozzle?
PETG is sticky when melted. If the nozzle is pressed too close to the bed it scrapes plastic up and drags blobs around. Raise the first layer very slightly, keep the nozzle clean, and dry the filament.
Get The First Layer, free every week
One short, friendly email a week: one fix or lesson, one honest pick, and one fun thing to print. New subscribers get the free First Print Checklist.
No spam, unsubscribe any time. See our privacy policy.