Last updated:
How to fix pillowing, holes and rough top surfaces on 3D prints
The walls look great, but the flat top of your print is bumpy, has little holes between the lines, or shows the infill grid underneath. That is called pillowing, and it is almost always a slicer problem rather than a broken printer. Work down this list in order and change one thing at a time.
How to recognize pillowing
- Small holes or gaps between the lines on a flat top surface
- Puffy bumps or dips, usually worst in the middle of large flat tops
- The infill pattern (grid, gyroid and so on) showing through the top
- Walls, corners and the bottom of the print look fine
If the walls are also thin, gappy or weak, the problem is probably not pillowing but under-extrusion, which shows up everywhere on the print. Start there instead.
Why it happens
The inside of most prints is sparse infill: mostly air with a pattern of lines holding it up. Prusa explains that the first solid top layer is essentially bridging over the infill pattern, so you will almost always see some sag in the first few solid lines. The lower the infill, the longer each little bridge, and the bigger the sag. Each layer printed on top fills in the dips of the one below. With too few layers, too little support underneath or too little cooling, the dips never get fully covered and you see them on the finished part.
Step 1: Check where it is and which profile you used
- Only on top? If it is only on flat tops, keep going with this guide. If it is everywhere, see under-extrusion first.
- Right profile? Make sure the slicer has your actual printer, nozzle size and filament selected. A profile for a different filament or nozzle can change flow, cooling and speed all at once.
- Look at the preview. Slice the model and scroll the layer slider to the top. You should see several layers of solid fill above the infill. If you only see one or two, that is your answer: go to step 2.
Step 2: Add top layers (the most common fix)
More solid layers on top give the surface a chance to cover the sag from the first ones. Prusa suggests at least 3 top layers, and points out that thin layers need more of them to reach the same thickness: about 3 layers at 0.3 mm layer height but about 9 layers at 0.1 mm. Prusa's own comparison photo shows the top getting smoother going from 1 to 2, 3 and 5 top layers.
- Bambu Studio: in the process settings, find Top shell layers and Top shell thickness (Strength tab). The two work together: Bambu Studio's own tooltip says that when the thickness from the layer count is thinner than the top shell thickness, the top shell layers will be increased. A Bambu Lab developer's example on GitHub: with 0.2 mm layers and a 1 mm top shell thickness, you get at least 5 top layers even if you typed 3.
- PrusaSlicer: Print Settings → Layers and perimeters → Solid layers → Top, plus a minimum shell thickness. The note under those boxes shows the resulting top thickness, so you can see the effect before you print.
Add one or two layers at a time and print a small test with a flat top. If the infill still shows through after a couple of extra layers, move on to step 3.
Step 3: Give the top layers something to sit on
Prusa says the main purpose of infill is to provide internal support for the top layers, which would otherwise have to bridge over empty space. Most models print fine at 10 to 15% infill, and you will rarely need more than 30%. If you dropped the infill very low to save time or filament, the top layers have much longer gaps to span.
- Raise the infill a little if it is well under 10%, or add more top layers to make up for very low infill.
- Denser infill only under the top: Prusa suggests a modifier that increases the infill for the last few layers before the solid top. Bambu Studio supports modifiers too, so you can raise infill just in that region instead of the whole part.
- Lightning infill is built for this: Prusa and Bambu Lab both describe it as getting denser under the top surface. It is fine for decorative parts but not for load-bearing ones. See best infill pattern and percentage for the trade-offs.
One fix a week, in plain English
Join The First Layer, our free beginner email. Each issue solves one common problem like this one. New subscribers get the free First Print Checklist.
No spam, unsubscribe any time. See our privacy policy.
Step 4: Check the cooling
Because the first top layers act like small bridges, they need to firm up quickly. Prusa's cooling guide says that for bridges and overhangs the plastic needs to freeze in place as soon as possible, otherwise it sags, and that bridge fan speed is usually set higher than for normal printing.
- Make sure the part cooling fan actually spins and the duct is not blocked or cracked. A fan that has stopped is an easy-to-miss cause of droopy tops and droopy overhangs at the same time.
- Don't turn the fan down on PLA without a reason. Your filament profile's cooling settings are a good starting point.
- ABS, ASA and PC are different. Prusa notes these materials are normally printed without the fan always on, because strong cooling can cause warping or layer splitting. With them, add top layers rather than cranking the fan. Our ABS and ASA guide covers why.
Step 5: Rule out low flow
If the top lines don't quite touch each other even on the last layer, the printer may simply be putting out a little too little plastic. Bambu Lab's flow rate guide says a flow rate that is too low causes gaps between printed lines, and lists rough or uneven surfaces as a sign the flow may be off.
- Dry the filament and clean the nozzle first. Bambu Lab says to make sure the filament is thoroughly dried and the hotend and extruder are clean before calibrating, or the result will be unreliable. See how to dry filament and how to fix a clogged nozzle.
- Run a flow rate calibration. In Bambu Studio it is under Calibration → Flow Rate. Auto calibration is X1-series only; other printers use manual mode, which prints a set of test blocks (coarse: 80 to 120% in 5% steps, then fine: 1% steps). Our flow rate and pressure advance calibration guide walks through it step by step.
- Pick the smoothest block. Bambu Lab's advice is to avoid any sample that shows even slight gaps between lines, because slight under-extrusion can grow into visible gaps on bigger prints. Save the result to your filament preset.
Step 6: Use a monotonic top pattern
The pattern of the very top layer changes how it looks. Prusa says its official profiles already use Monotonic as the top layer pattern, and PrusaSlicer's Top fill pattern setting changes only the visible top layer, not the solid layers below it. Bambu Studio also prints the sub-top surface (the single layer right under the top) with Monotonic by default; Bambu Lab says this reduces marks from the internal solid infill showing through on the top surface. If you have changed these patterns, try setting them back to Monotonic.
Step 7: Iron flat tops for a smooth finish
Ironing runs the hot nozzle back over the finished top layer at the same height with a very small amount of flow. The heat flattens the lines and the extra plastic fills small gaps. Prusa's comparison photos show a visibly smoother top with ironing on.
- Bambu Studio: set Ironing type (off by default) to Top surfaces (every flat top) or Topmost surface (only the very last layer). All solid layer is rarely needed and adds a lot of time.
- PrusaSlicer: switch to Advanced or Expert mode, then Print Settings → Infill → Ironing → Enable ironing. Ironing speed is in a different place: Print Settings → Speed → Ironing.
- Tuning: both makers say slower ironing usually works better. Ironing flow too high leaves excess plastic dragged to the edges; too low leaves shiny grooves. Line spacing should be smaller than your nozzle diameter. If plastic builds up at the edges, Bambu Studio (1.10 and later) has an Ironing inset setting to keep the nozzle back from the edge.
Know the downsides before you turn it on everywhere:
- It is slower. Large flat tops can add a lot of print time.
- Clog risk. Slow, tiny extrusion can cause heat creep and a blocked hotend. Bambu Lab mentions PLA, PETG and TPU; Prusa says PLA is most prone, especially in hot weather.
- Adhesion matters. Bambu Lab warns the nozzle rubs on the top layer, so a part that isn't stuck down firmly can be knocked off.
- Flat, level tops only. Both makers say ironing does little on curved or sloped tops, figures and organic shapes; it just adds time.
Ironing smooths a top that is already solid. If the top is full of holes, fix steps 2 to 5 first. Another option from Prusa: if the model allows it, print it upside down. The face printed on the build plate is typically even smoother than an ironed top.
Holes on sloped or rounded tops
Holes on the top of a dome, a figure's head or a gentle slope are a slightly different problem. Prusa describes holes between perimeters on slanted surfaces as a classic issue with busts and organic models, and its fix is Ensure vertical shell thickness, which adds solid infill near sloping surfaces. Keep it on its standard Enabled setting in PrusaSlicer (Prusa notes the option was not available in versions 2.6.0 to 2.8.1). Bambu Studio has a setting with the same name in its strength settings. Adding top layers also helps here.
Quick reference: what you see and what to change
| What you see | Most likely cause | Go to |
|---|---|---|
| Infill grid showing through a flat top | Too few top layers | Step 2 |
| Holes and dips, worse with very low infill | Top layers bridging long gaps | Steps 2 and 3 |
| Droopy top lines and droopy overhangs | Weak or stopped part cooling | Step 4 |
| Top lines don't touch, walls also thin | Low flow or under-extrusion | Step 5 |
| Solid top but streaky, with marks from below | Top or sub-top pattern changed | Step 6 |
| Solid top, you just want it smoother | Normal FDM lines | Step 7 (ironing) |
| Holes only on a dome, head or slope | Thin shell on sloped surfaces | Ensure vertical shell thickness |
Sources
Checked November 14, 2026: Prusa Knowledge Base, Layers and perimeters, Infill, Cooling and Ironing; Bambu Lab Wiki, Ironing, Flow Rate Calibration and Strength Advanced Setting; Bambu Studio GitHub, issue 3872 (top shell layers vs top shell thickness).
Your next step
Top surfaces smooth again? To understand the rest of the slicer screen, read slicer settings explained. If the sides of your prints now show ripples after corners, see how to fix ghosting and ringing, and for stripes around the walls, how to fix Z-banding.
Frequently asked questions
What is pillowing in 3D printing?
Pillowing is when the flat top of a print comes out bumpy, with small dips, puffy bulges or holes between the lines, a bit like the surface of a pillow. It happens because the first solid top layers are printed over sparse infill and have to bridge the air between the infill lines. They sag a little, and if there are not enough layers on top, the sag never gets covered.
How many top layers do I need?
Prusa suggests at least 3 top layers, and more when you print thin layers so the total thickness stays the same: about 3 layers at a 0.3 mm layer height but about 9 at 0.1 mm. In Bambu Studio and PrusaSlicer you can also set a minimum top thickness in millimeters; the slicer adds layers if the layer count alone would be thinner than that.
Will ironing fix pillowing?
Only partly. Ironing runs the hot nozzle over the finished top layer with a tiny amount of flow to fill small gaps and flatten the lines, so it smooths a top that is already solid. It does not add the thickness that covers sagging over the infill, and Bambu Lab and Prusa both note that it adds print time and can raise the risk of heat-creep clogs. Fix the top layers, infill and cooling first, then iron if you want a smoother finish.
Why do I see the infill pattern through the top of my print?
There is not enough solid material on top of the infill. The usual fixes are more top layers (or a higher top shell thickness), a slightly higher infill percentage, and good cooling for the first top layers. If the walls also look thin and gappy, the real cause is probably under-extrusion.
Why does the top of my print have holes but the walls look fine?
That usually points to the top-surface settings rather than the printer: too few top layers, very low infill, or weak cooling on the first top layers. If the holes are on a sloped or rounded top, like the top of a head on a figure, make sure Ensure vertical shell thickness is switched on in your slicer.
Get The First Layer, free every week
One short, friendly email a week: one fix or lesson, one honest pick, and one fun thing to print. New subscribers get the free First Print Checklist.
No spam, unsubscribe any time. See our privacy policy.